Turning demolition waste into sand and stone: a short account of a mobile sensor-controlled recycling line

##article.authors##

  • Duong Van Sinh Institute for Applied Blockchain Technology, Legal Studies and Intellectual Property, Ho Chi Minh City, Vietnam; Institute for Natural Disaster and Environmental Research (RIDES), HCMC Branch, 38 D15A, Phuoc Long, Ho Chi Minh City, Vietnam

DOI:

https://doi.org/10.31224/8836

Keywords:

construction and demolition waste, recycled aggregate, artificial sand, mobile recycling, sensor control, circular economy

Abstract

Demolition waste is usually landfilled or dumped, while natural river sand grows scarce. Crushing demolition waste alone rarely yields stable aggregate, and its grading drifts with the feedstock. This short paper describes a mobile, sensor-controlled recycling line: vibrating feeder with manual picking, belt magnet, jaw crusher and vertical-shaft impactor, multi-deck screen with oversize recirculation, and water-cyclone washing with recirculation and sludge recovery. Sensors for flow, turbidity and particle size adjust feed, rotor speed, water and screening. The design reference is about 100 tonnes per day (12.5 tonnes per hour on a single 8-hour shift), with 20/10/5 mm screen apertures, a 75 mm jaw setting, a 60 m/s rotor tip speed and a 63 µm cyclone cut. It targets sand 0–5 mm and stone 5–10 and 10–20 mm; a 20–40 mm band is claimed in the dossier, but the reference line as described is not configured to produce it — that would need an additional screen deck. No pilot has been run. No measured product properties, pilot throughput, energy use, or water use are reported — none exist in the dossier. All performance figures are simulated estimates: about 90.3 tonnes per day of saleable product from 100 tonnes of feed, simulated electricity use of 3.7 kWh per tonne of feed, fresh make-up water of 0.16 m³ per tonne of feed at 93% recirculation, and simulated 28-day concrete strengths of 36.0 MPa at 20% coarse replacement and 27.0 MPa at 100% coarse replacement, against a 38.0 MPa reference.

Downloads

Download data is not yet available.

Downloads

Posted

2026-11-19